Inquiry
K477 (K77) Alloy Powder
Catalog | ACAM-AP-A045 |
Description | K477 (K77) alloy is characterized by high strength and plasticity and good casting process performance. It is suitable for making high-temperature parts such as the outer ring of aviation gas turbine working below 900 °C. |
Density | 7.95 g/cm3 |
Application | Selective laser melting (SLM) Feedstock for additive manufacturing processes such as electron beam melting (EBM) Additives for special applications |
Feature | High powder sphericity, smooth surface, high material purity, low oxygen content, uniform particle size distribution, good flowability, high apparent density, high vibration density |
Melting Temperature | 1210-1290 °C |
Morphology | Spherical |
Packing Type | As per customer requirement |
Particle Size | 5-15 μm, 15-45 μm, 15-53 μm, 45-105 μm, 45-150 μm, or customizable |
Processing Method | Atomization |
Storage Conditions | K477 (K77) alloy powder should be well sealed and stored in a cool and dry place, avoiding direct light. |